Axiall 2161A Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 2161A Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant, oil resistant, 105°C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 83 - 89
83 - 89
delayed; ASTM D-2240
Tensile Strength, Yield 16.9 MPa
2450 psi
ASTM D-638
Elongation at Yield 273 %
273 %
Oil Aging: 96 hours @ 100°C; #2 Oil; 30 mil slabs; UL 1581
285.3 %
285.3 %
Air Aging: 7 days @ 136°C; 30 mil slabs; UL 1581
350 %
350 %
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -14.0 °C
6.80 °F
ASTM D-746
Oxygen Index 29 %
29 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F