Polymer Property : Brittleness Temperature = -67.8 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -67.8 °C
-90.0 °F
ASTM 746
ExxonMobil Vyram™ 9101-55 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Brittleness Temperature -67.8 °C
-90.0 °F
Ethylene Propylene Rubber (EPM, EPDM)
Satisfactory compatibility with fireproof hydraulic fluids, ketones, hot and cold water, alkalis, and ozone/strong oxidizing chemicals. Unsatisfactory compatibility with most oils, gasoline, kerosen..
Brittleness Temperature -67.8 °C
-90.0 °F
ASTM D746; ISO 812
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer
DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent soft touch feel a..
Brittleness Temperature -67.8 °C
-90.0 °F
ASTM D746; ISO 812
Advanced Polymer Alloys DuraGrip™ 6170 BK Melt Processable Elastomer
DuraGrip™ 6170BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6170BK has an excellent soft touch feel a..
Brittleness Temperature -67.8 °C
-90.0 °F
ASTM D746; ISO 812
Advanced Polymer Alloys DuraGrip™ DGR 6050 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6050 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6050 NC/BK have an excellent soft t..
Brittleness Temperature -67.8 °C
-90.0 °F
ASTM 746
ExxonMobil Vyram™ 9201-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..