Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -67.8 °C | -90.0 °F | ASTM 746 |
ExxonMobil Vyram™ 9101-55 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Brittleness Temperature | -67.8 °C | -90.0 °F | |
Ethylene Propylene Rubber (EPM, EPDM) Satisfactory compatibility with fireproof hydraulic fluids, ketones, hot and cold water, alkalis, and ozone/strong oxidizing chemicals. Unsatisfactory compatibility with most oils, gasoline, kerosen.. |
|||
Brittleness Temperature | -67.8 °C | -90.0 °F | ASTM D746; ISO 812 |
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent
soft touch feel a.. |
|||
Brittleness Temperature | -67.8 °C | -90.0 °F | ASTM D746; ISO 812 |
Advanced Polymer Alloys DuraGrip™ 6170 BK Melt Processable Elastomer DuraGrip™ 6170BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6170BK has an excellent
soft touch feel a.. |
|||
Brittleness Temperature | -67.8 °C | -90.0 °F | ASTM D746; ISO 812 |
Advanced Polymer Alloys DuraGrip™ DGR 6050 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6050 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6050 NC/BK have
an excellent soft t.. |
|||
Brittleness Temperature | -67.8 °C | -90.0 °F | ASTM 746 |
ExxonMobil Vyram™ 9201-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |