Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glow Wire Test = 925 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glow Wire Test 925 °C

@Thickness 1.50 mm
1700 °F

@Thickness 0.0591 in
GWFI; IEC 60695-2-12
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Glow Wire Test 925 °C

@Thickness 2.00 mm
1700 °F

@Thickness 0.0787 in
GWFI; IEC 60695-2-12
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Glow Wire Test 925 °C

@Thickness 1.50 mm
1700 °F

@Thickness 0.0591 in
GWFI; IEC 60695-2-12
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized
Information provided by Polymer Technology and Services, LLC (PTS).
Glow Wire Test 925 °C

@Thickness 2.00 mm
1700 °F

@Thickness 0.0787 in
GWFI; IEC 60695-2-12
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized
Information provided by Polymer Technology and Services, LLC (PTS).
Glow Wire Test 925 °C

@Thickness 1.50 mm
1700 °F

@Thickness 0.0591 in
Ignition; IEC 60695-2-13
DuPont Performance Polymers Rynite® GW520CS NC010 PET  (Unverified Data**)
Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Glow Wire Test 925 °C

@Thickness 3.00 mm
1700 °F

@Thickness 0.118 in
Ignition; IEC 60695-2-13
DuPont Performance Polymers Rynite® GW520CS NC010 PET  (Unverified Data**)
Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Glow Wire Test 925 °C

@Thickness 1.00 mm
1700 °F

@Thickness 0.0394 in
GWIT
LATI Latiohm 87/26-06 PD01-V1 PC, Flame Retardant
Semiconductive/dissipative product based on Polycarbonate (PC). UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Glow Wire Test 925 °C

@Thickness 2.00 mm
1700 °F

@Thickness 0.0787 in
GWIT
LATI Latiohm 87/26-06 PD01-V1 PC, Flame Retardant
Semiconductive/dissipative product based on Polycarbonate (PC). UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Glow Wire Test 925 °C

@Thickness 2.00 mm
1700 °F

@Thickness 0.0787 in
(GWIT); IEC 60695-2-13
Styron EMERGEâ„¢ 7560 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7560 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..
Glow Wire Test 925 °C

@Thickness 3.00 mm
1700 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Glow Wire Test 925 °C

@Thickness 3.00 mm
1700 °F

@Thickness 0.118 in
Glow Wire Flammability Index; IEC 60695-2-12
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
Glow Wire Test 925 °C

@Thickness 3.00 mm
1700 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Glow Wire Test 925 °C

@Thickness 3.00 mm
1700 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Glow Wire Test 925 °C

@Thickness 3.00 mm
1700 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Glow Wire Test 925 °C

@Thickness 3.00 mm
1700 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Glow Wire Test 925 °C

@Thickness 2.00 mm
1700 °F

@Thickness 0.0787 in
GWIT; IEC 60695
Eurotec® Tecotek® PC44 GR003 ZG70 PC, unfilled, flame retardant - halogen (RoHS compliant), light grey
Information provided by Eurotec®
Glow Wire Test 925 °C

@Thickness 0.750 mm
1700 °F

@Thickness 0.0295 in
DAM; Ignition; IEC 60695-2-13
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P..
Glow Wire Test 925 °C

@Thickness 1.50 mm
1700 °F

@Thickness 0.0591 in
DAM; Ignition; IEC 60695-2-13
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P..
Glow Wire Test 925 °C

@Thickness 3.00 mm
1700 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..