Polymer Property : Beta Transus = 1015 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Beta Transus 1015 °C
1859 °F
TIMET TIMETAL® 1100 Titanium Alloy (Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si)
Features: A near alpha, high temperature creep resistant alloy developed for elevated temperature use in the range of 600°C that offers the highest combination of strength, creep resistance, fractu..
Beta Transus 1015 °C
1859 °F
TIMET TIMETAL® 829 (Ti-5.5Al-3.5Sn-3Zr-1Nb-0.25Mo-0.3Si) Titanium Alloy
Weldable, High Strength, High Temperature, Creep Resistant AlloyFeatures: TIMETAL 829 combines creep resistance up to 540°C with good oxidation resistance. It is weldable and like TIMETAL 685, TIME..
Beta Transus 1015 °C
1859 °F
TIMET TIMETAL® 367 (Ti-6Al-7Nb) Titanium Alloy
Medium-Strength Surgical Implant AlloyFeatures: TIMETAL 367 is a dedicated, medium strength, titanium alloy for surgical implants. The alloy was developed specifically for the manufacture of femora..