Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 - 146 °C
178 - 295 °F
Average value: 94.5 °C Grade Count:19
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
Deflection Temperature at 1.8 MPa (264 psi) 98.9 - 146 °C
210 - 295 °F
Average value: 108 °C Grade Count:22
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu..
Deflection Temperature at 1.8 MPa (264 psi) 131 - 146 °C
268 - 295 °F
Average value: 137 °C Grade Count:10
Overview of materials for Polycarbonate, Foam Grade, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum ..
Deflection Temperature at 1.8 MPa (264 psi) 51.0 - 146 °C
124 - 295 °F
Average value: 69.8 °C Grade Count:13
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a..