Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C @Thickness 6.40 mm |
304 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C @Thickness 3.20 mm |
304 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP 9X06483 PA 46 LNP* Lubricomp* 9X06483 is a compound based on a Nylon 4/6 containing PTFE. Added feature of this grade is: Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C @Thickness 3.20 mm |
304 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3220A PP SABIC® PPcompound G3220A is a general purpose, 20% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS is 209767996. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 304 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers PrimoSpire® PR-250 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-250 resin is an injection molding grade of self-reinforced polyphenylene (SRP). PrimoSpire® SRP is an ultra-high performance amorphous, melt-processable polymer. The unique prop.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C @Thickness 6.40 mm |
304 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 457 PBT 6.5% GR PBT, UL94 V-0/5V. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C @Thickness 6.40 mm |
304 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 457 PBT (Asia Pacific) 6.5% GR PBT, UL94 V-0/5V. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 304 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp GX061104 PSU (Europe-Africa-Middle East) LNP* COLORCOMP* GX061104 is a compound based on Polysulfone resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C @Thickness 3.20 mm |
304 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP MX00709 PP LNP* THERMOCOMP* MX00709 is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this grade are: Heat Stabilized, UV Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C @Thickness 3.20 mm |
304 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C @Thickness 6.40 mm |
304 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl 534 PPE+PS High heat, unreinforced.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 304 °F | ASTM D648 |
Plenco 7500 Phenolic, Granular, Injection Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 304 °F | ISO 75-1, 2 |
Polyplastics TOPAS® 6017 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Possesses the highest heat resistance among cyclic olefin-type resins.Information provided by PolyPlastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 304 °F | ASTM-D648 |
Polyram Polytron P40B03 Copolymer Polypropylene, Chemically Coupled 40% Long Glass Fiber A CHEMICALLY COUPLED 40% LONG GLASS FIBERS REINFORCED BLACK POLYPROPYLENE, HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteris.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 304 °F | ISO 75 |
Polyram Polytron P40N03 Polypropylene, 40% Long Glass Fibers Is a chemically coupled 40% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance ch.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 304 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Af |
Eurostar Starglas GX061104 PSU Starglas GX061104 is a PSU resin (also known as Starglas PSU A ¾)Information provided by Eurostar. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 304 °F | ASTM D648 |
Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 303 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-25FG-0687 25% Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 304 °F | ASTM D648 |
A. Schulman ComAlloy Aqualoy® 140 Polypropylene, Glass Reinforced, Chemically Coupled NSF Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 304 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 304 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL FE8000S PPE+PS Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 304 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 151 °C | 303 °F | Unannealed; ASTM D648 |
LyondellBasell Hostacom™ PF062-3 Polypropylene Homopolymer Description: Hostacom™ PF062-3 high melt flow, 5,200 MPa flexural modulus, chemically coupled, 30% glass fiber-reinforced polypropylene homopolymer has good impact strength, high stiffness and very.. |