Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 71.0 - 175 °C
160 - 347 °F
Average value: 100 °C Grade Count:67
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Deflection Temperature at 1.8 MPa (264 psi) 155 - 175 °C
311 - 347 °F
ISO 75 Af
Vyncolit 4221 XB Novolac Phenolic
Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group
Deflection Temperature at 1.8 MPa (264 psi) 155 - 175 °C
311 - 347 °F
ISO 75 A
Vyncolit 4451 XB Novolac Phenolic
Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a..
Deflection Temperature at 1.8 MPa (264 psi) 141 - 175 °C
286 - 347 °F
Average value: 164 °C Grade Count:3
Overview of materials for PEKK, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate..
Deflection Temperature at 1.8 MPa (264 psi) 65.0 - 175 °C
149 - 347 °F
Average value: 149 °C Grade Count:125
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
Deflection Temperature at 1.8 MPa (264 psi) 85.0 - 175 °C
185 - 347 °F
Average value: 154 °C Grade Count:17
Overview of materials for Polypropylene with 60% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i..