Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 184 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral filled PA6 compound
Deflection Temperature at 1.8 MPa (264 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP EX00548C PEI
LNP LUBRICOMP* EX00548C is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Clean Compounding System, Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 184 °C

@Thickness 6.40 mm
363 °F

@Thickness 0.252 in
unannealed; ASTM D 648
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 184 °C

@Thickness 6.40 mm
363 °F

@Thickness 0.252 in
unannealed; ASTM D 648
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Deflection Temperature at 1.8 MPa (264 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP STAT-KON WSF42 PBT (Europe-Africa-Middle East)
LNP*STAT-KON* WSF42 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Stainless Steel Fiber. Added features include: Electrically Conductive.
Deflection Temperature at 1.8 MPa (264 psi) 184 °C

@Thickness 3.20 mm
363 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP YF002 POLYESTER ELASTOMER
LNP* THERMOCOMP* YF002 is a compound based on Poyester Elastomer containing 10% Glass Fiber. Added feature of this grade is: High Modulus.
Deflection Temperature at 1.8 MPa (264 psi) 184 °C

@Thickness 6.40 mm
363 °F

@Thickness 0.252 in
unannealed; ASTM D 648
SABIC Innovative Plastics Ultem ATX152R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 1.8 MPa (264 psi) 184 °C
363 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
SABIC Innovative Plastics Ultem LTX931A PEI Blend (Europe-Africa-Middle East)
Post-industrial recycle based, 30% glass fiber filled, high flow Polyetherimide blend. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Deflection Temperature at 1.8 MPa (264 psi) 184 °C
363 °F
80*10*4 s=60mm; ISO 75-1 a
Sax Polymers SAXAMID 126F2K4 Nylon 6, Glass Fiber/Bead Filled
SAXAMID 126F2K4 is a 10% glass fibers and 20% glass beads filled polyamide 6 injection-molding-grade.Information provided by SAX Polymers
Deflection Temperature at 1.8 MPa (264 psi) 184 °C
363 °F
ASTM D648
Plenco 00755 Melamine-Phenolic, Granular, Compression Molded
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755..
Deflection Temperature at 1.8 MPa (264 psi) 184 °C
363 °F
ISO 75
BASF Ultradur B 4300 G2 LS High Speed BK15045 10% Glass Filled PBT
Deflection Temperature at 1.8 MPa (264 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOTUF VX99810 Super Tough Nylon
Super Tough Nylon, Proprietary Filler(s),