Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 193.0 °C | 379.4 °F | Unannealed; ASTM D648 |
PolyOne Nymax™ GF 1880 33 HS NATURAL Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedHeat StabilizedMolded Test Bars: (Dry as molded:Information provided by PolyOne Corporation. |