Deflection Temperature at 1.8 MPa (264 psi) 193.0 °C
379.4 °F
Unannealed; ASTM D648
PolyOne Nymax™ GF 1880 33 HS NATURAL Nylon 6/12, Glass Filled  (discontinued **)