Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 48.9 - 210 °C
120 - 410 °F
Average value: 78.9 °C Grade Count:49
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Deflection Temperature at 1.8 MPa (264 psi) 120 - 210 °C
248 - 410 °F
Average value: 149 °C Grade Count:17
Overview of materials for Polyphenylene Ether, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ..
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 210 °C
122 - 410 °F
Average value: 169 °C Grade Count:8
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum..
Deflection Temperature at 1.8 MPa (264 psi) 62.8 - 210 °C
145 - 410 °F
Average value: 72.8 °C Grade Count:19
Overview of materials for ECTFE Fluoropolymer
This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat..
Deflection Temperature at 1.8 MPa (264 psi) 82.2 - 210 °C
180 - 410 °F
Average value: 159 °C Grade Count:5
Overview of materials for Nylon 6, Stainless Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o..
Deflection Temperature at 1.8 MPa (264 psi) 55.0 - 210 °C
131 - 410 °F
Average value: 101 °C Grade Count:29
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..