Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 - 98.9 °C | 176 - 210 °F | Average value: 90.3 °C Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 - 98.9 °C | 172 - 210 °F | Average value: 90.6 °C Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 - 98.9 °C | 170 - 210 °F | Average value: 87.7 °C Grade Count:14 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 41.0 - 99.0 °C | 106 - 210 °F | Average value: 53.7 °C Grade Count:20 |
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Rotational Molding Grade". Each property range of values reported is m.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.1 - 98.9 °C | 169 - 210 °F | Average value: 91.9 °C Grade Count:4 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 - 98.9 °C | 104 - 210 °F | Average value: 77.5 °C Grade Count:54 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |