Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA)

Category Polymer , Thermoplastic , Polystyrene (PS) , Styrene/Methyl Methacrylate Copolymer (SMMA)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.03 - 1.13 g/cc
0.0372 - 0.0408 lb/in³
Average value: 1.07 g/cc Grade Count:13
Water Absorption 0.100 - 1.00 %
0.100 - 1.00 %
Average value: 0.196 % Grade Count:10
Linear Mold Shrinkage 0.00200 - 0.00600 cm/cm
0.00200 - 0.00600 in/in
Average value: 0.00400 cm/cm Grade Count:12
Melt Flow 0.400 - 26.9 g/10 min
0.400 - 26.9 g/10 min
Average value: 4.70 g/10 min Grade Count:13
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75.0 - 85.0
75.0 - 85.0
Average value: 79.3 Grade Count:3
Hardness, Shore D 69.0 - 75.0
69.0 - 75.0
Average value: 72.0 Grade Count:4
Tensile Strength, Ultimate 25.5 - 65.5 MPa
3700 - 9500 psi
Average value: 43.7 MPa Grade Count:9
Tensile Strength, Yield 57.2 - 85.0 MPa
8300 - 12300 psi
Average value: 68.7 MPa Grade Count:4
Elongation at Break 2.30 - 54.0 %
2.30 - 54.0 %
Average value: 18.6 % Grade Count:13
Modulus of Elasticity 2.20 - 3.45 GPa
319 - 501 ksi
Average value: 2.96 GPa Grade Count:6
Flexural Modulus 1.58 - 3.16 GPa
229 - 458 ksi
Average value: 2.44 GPa Grade Count:11
Izod Impact, Notched 0.160 - 0.481 J/cm
0.300 - 0.900 ft-lb/in
Average value: 0.274 J/cm Grade Count:12
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 - 100 °C
169 - 212 °F
Average value: 85.1 °C Grade Count:9
Deflection Temperature at 1.8 MPa (264 psi) 76.1 - 98.9 °C
169 - 210 °F
Average value: 91.9 °C Grade Count:4
Vicat Softening Point 92.0 - 103 °C
198 - 217 °F
Average value: 98.2 °C Grade Count:11
Optical Properties Metric English Comments
Transmission, Visible 80.0 - 92.0 %
80.0 - 92.0 %
Average value: 88.8 % Grade Count:11