Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 218 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 190 - 218 °C
374 - 425 °F
Average value: 207 °C Grade Count:62
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 218 °C
140 - 425 °F
Average value: 199 °C Grade Count:130
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Deflection Temperature at 1.8 MPa (264 psi) 79.4 - 218 °C
175 - 424 °F
Average value: 192 °C Grade Count:18
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..