Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.8 - 113 °C
145 - 235 °F
Average value: 85.4 °C Grade Count:21
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..