Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 37.0 °C
98.6 °F
ASTM D648-95
Multibase Multi-Pro® 0001 Black Polypropylene
This product was specially designed for one customer's extrusion application needs. Data is taken from sample material only.Data provided by Multibase.
Deflection Temperature at 1.8 MPa (264 psi) 37.0 °C
98.6 °F
ASTM D648
ExxonMobil Escorene® LL-8361 LLDPE, Rotational Molding Powder  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-8 type protection, Good flowUses: Consumer items, Potable water tanks, Laundry tubs
Deflection Temperature at 1.8 MPa (264 psi) 37.0 °C
98.6 °F
ASTM D648
ExxonMobil LL 8360.29 Rotational Molding Resin
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui..
Deflection Temperature at 1.8 MPa (264 psi) 37.0 °C
98.6 °F
ASTM D648
ExxonMobil LLP8360.29 Rotational Molding Resin
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui..
Deflection Temperature at 1.8 MPa (264 psi) 37.0 °C
98.6 °F
ASTM D648
ExxonMobil LL 8360 Rotational Molding Resin  (discontinued **)
LL 8360 is a linear low density hexene copolymer designed to provide good processability along with outstanding dimensional control and low warpage. This resin is ideally suited for applications tha..
Deflection Temperature at 1.8 MPa (264 psi) 37.0 - 41.0 °C
98.6 - 106 °F
Average value: 38.5 °C Grade Count:25
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report..
Deflection Temperature at 1.8 MPa (264 psi) 37.0 - 42.0 °C
98.6 - 108 °F
Average value: 39.1 °C Grade Count:7
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i..
Deflection Temperature at 1.8 MPa (264 psi) 37.0 °C
98.6 °F
ASTM D648
ExxonMobil Escorene® LL-8302 LMDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8302 is the base re..
Deflection Temperature at 1.8 MPa (264 psi) 37.0 °C
98.6 °F
ASTM D648
ExxonMobil Escorene® LL-8361 LMDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8361 is fully formu..