Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 37.0 °C | 98.6 °F | ASTM D648-95 |
Multibase Multi-Pro® 0001 Black Polypropylene This product was specially designed for one customer's extrusion application needs. Data is taken from sample material only.Data provided by Multibase. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.0 °C | 98.6 °F | ASTM D648 |
ExxonMobil Escorene® LL-8361 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-8 type protection, Good flowUses: Consumer items, Potable water tanks, Laundry tubs |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.0 °C | 98.6 °F | ASTM D648 |
ExxonMobil LL 8360.29 Rotational Molding Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.0 °C | 98.6 °F | ASTM D648 |
ExxonMobil LLP8360.29 Rotational Molding Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.0 °C | 98.6 °F | ASTM D648 |
ExxonMobil LL 8360 Rotational Molding Resin
(discontinued **) LL 8360 is a linear low density hexene copolymer designed to provide good processability along with outstanding dimensional control and low warpage. This resin is ideally suited for applications tha.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.0 - 41.0 °C | 98.6 - 106 °F | Average value: 38.5 °C Grade Count:25 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.0 - 42.0 °C | 98.6 - 108 °F | Average value: 39.1 °C Grade Count:7 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.0 °C | 98.6 °F | ASTM D648 |
ExxonMobil Escorene® LL-8302 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8302 is the base re.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.0 °C | 98.6 °F | ASTM D648 |
ExxonMobil Escorene® LL-8361 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8361 is fully formu.. |