Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LL 8360.29 Rotational Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LL 8360.29 Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally suited for applications that require excellent processability and ESCR along with the optimum balance of stiffness and low temperature toughness. Availability: Latin America, North America and South America Additive: Stabilizer: YesLong Term UV-15 Applications: Agricultural Tank LinersConsumer ArticlesExternally supported intermediate bulk containersLarge Sized Industrial Parts Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.932 g/cc
0.0337 lb/in³
ASTM D4883
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
ASTM D1693
ESCR 10% Igepal® 650 hour
650 hour
ASTM D1693
Melt Flow 5.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.2 MPa
2200 psi
(2.0 in/min); ASTM D638
Elongation at Yield 20 %
20 %
(2.0 in/min); ASTM D638
Flexural Modulus 0.600 GPa
87.0 ksi
1% secant; ASTM D790
Impact Test 88.1 J

@Thickness 3.17 mm,
Temperature -40.0 °C
65.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
217 J

@Thickness 6.35 mm,
Temperature -40.0 °C
160 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
Thermal Properties Metric English Comments
Melting Point 125 °C
257 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C
131 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 37.0 °C
98.6 °F
ASTM D648
Descriptive Properties Value Comments
Features long term UV 8 stabilization
Form PELLET
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved