Material Notes:
DuPont Vespel TP-8395 parts are specified for high-temperature and high-wear applications. TP-8395 parts offer an excellent balance of mechanical and thermal properties for superior performance in aggressive environments. TP-8395 parts are produced from fInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Water Absorption 0.20 %

@Temperature 23.0 °C
0.20 %

@Temperature 73.4 °F
Immersion 24h; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength 73.0 MPa

@Temperature 23.0 °C
10600 psi

@Temperature 73.4 °F
ASTM D638
Flexural Strength 117 MPa

@Temperature 23.0 °C
17000 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 0.00260 GPa

@Temperature 23.0 °C
0.377 ksi

@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 0.780 J/cm

@Temperature 23.0 °C
1.46 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 52.0 µm/m-°C

@Temperature 23.0 - 150 °C
28.9 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 228
CTE, linear, Transverse to Flow 49.0 µm/m-°C

@Temperature 23.0 - 150 °C
27.2 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 228
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ASTM D648
Descriptive Properties Value Comments
Appearance Natural Color
Forms Shapes
Material Status Current
Region Available - Global Yes
RoHS Compliance Contact Manufacturer