Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 543 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 284 °C
543 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable..
Deflection Temperature at 1.8 MPa (264 psi) 284 °C
543 °F
MTI ThermoStran® PPA-50G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Deflection Temperature at 1.8 MPa (264 psi) 284 °C
543 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA
LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 284 °C

@Thickness 3.20 mm
543 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA
LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 284 °C
543 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to..
Deflection Temperature at 1.8 MPa (264 psi) 284 °C
543 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel..
Deflection Temperature at 1.8 MPa (264 psi) 284 °C
543 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont ..