Thermal Properties Metric English Comments
Softening Point 160 °C
320 °F
T5 Point - modulus = 690 MPa (100,000 psi)
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating
Parylene N, poly(para-xylylene), is a completely linear, highly crystalline material. Parylene N is a primary dielectric, exhibiting a very low dissipation factor, high dielectric strength, and a lo..
Softening Point 160 - 180 °C
320 - 356 °F
Sibur 1045-12 Compound 948 Polyvinyl Chloride (PVC)
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p..
Softening Point 160 - 180 °C
320 - 356 °F
Sibur O-40 Compound 239 Polyvinyl Chloride (PVC)
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p..
Softening Point 160 - 180 °C
320 - 356 °F
Sibur O-40 Compound OM-40 Polyvinyl Chloride (PVC)
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p..
Softening Point 160 - 180 °C
320 - 356 °F
Sibur O-55 Compound 1182 Polyvinyl Chloride (PVC)
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p..
Softening Point 160 °C
320 °F
JIS K-2531
Unitika elitel UE3203 Polyester, Pellet
High elongation type UE3200UNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binders,..
Softening Point 160 °C
320 °F
Valley Adhesives EM-490 High Temperature Application Glue Stick
Valley Adhesives EM-490 High Temperature Application Glue StickExcellent tack; Used on plastics, metals and other surfaces.
Softening Point 160 °C
320 °F
JIS K-2531
Unitika elitel UE3690 Polyester, Pellet
High Tg, PET adhesiveness, High heat resistance, BinderUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as ad..
Softening Point 160 - 190 °C
320 - 374 °F
Average value: 174 °C Grade Count:7
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..