Valley Adhesives EM-490 High Temperature Application Glue Stick

Category Polymer , Adhesive , Thermoset
Manufacturer Valley Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Valley Adhesives EM-490 High Temperature Application Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Valley Adhesives EM-490 High Temperature Application Glue StickExcellent tack; Used on plastics, metals and other surfaces.
Physical Properties Metric English Comments
Viscosity 1350 cP
1350 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Tensile Strength, Ultimate 1.56 MPa
226 psi
Elongation at Break 290 %
290 %
Shear Strength 2.03 MPa
294 psi
Peel Strength 5.64 kN/m
32.2 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Heat Resistance Value at 2 psi.
Softening Point 160 °C
320 °F
Processing Properties Metric English Comments
Cure Time 0.133 min
0.00222 hour
Hot tack
Pot Life 0.75 min
0.75 min
Open Time
Descriptive Properties Value Comments
Color Opaque