Blue River Coatings Hydro-Gloss 2-Part Polyurethane Top Coat

Category Polymer , Adhesive , Thermoset , Polyurethane, TS
Manufacturer Blue River Coatings
Trade Name Hydro-Gloss
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Blue River Coatings Hydro-Gloss 2-Part Polyurethane Top Coat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BLUE RIVER COATINGS HYDRO-GLOSS 2-PART POLYURETHANE TOPCOAT is a water dispersible polyisocyanate coating. HYDRO-GLOSS provides outstanding coverage, excellent durability, and ease of application as well as being a low VOC and EPA compliant coating. HYDRO-GLOSS offers superior adhesion and has film properties that rival most solvent based catalyzed polyurethane systems. Enviromental Advantages:BLUE RIVER COATINGS HYDRO-GLOSS 2-PART POLYURETHANE TOPCOAT is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling. Characteristics:Excellent exterior durabilityNon-photochemically reactiveFull gloss – 92% at 60° glossometerAvailable in satin to gloss finishExcellent hardness/impact resistanceExcellent adhesion, mar, and abrasion resistanceCoating will not flash rust on clean, dry metalsCoatings can be applied in a wide range of temperature and humidity conditions without the use of retardersLinear flexibility is excellent on substrates such as Lexan, vinyl, and fiberglassExcellent retention of gloss in 1,000 hour QUV weatherometerWater is used for reductionExcellent performance on most plasticsWater is used for clean-upNon-HazardousWide range of colorsShelf life of 1 yearNon-FlammableMetallics can be formulatedUsesSteel, Steel DecksAluminumVinylFiberglassWood PlasticsCanvasInformation provided by Blue River Coatings
Physical Properties Metric English Comments
Specific Gravity >= 1.00 g/cc
>= 1.00 g/cc
Density 1.13 g/cc
0.0407 lb/in³
Solids Content 47 %
47 %
by weight
50 %
50 %
by volume
Volatile Organic Compounds (VOC) Content 36 g/l
36 g/l
Mechanical Properties Metric English Comments
Impact Test 20.3 J
15.0 ft-lb
Forward and Reverse
Taber Abrasion, mg/1000 Cycles 100
100
CS17 wheel, 1000 g load
Thermal Properties Metric English Comments
Boiling Point 171 °C
340 °F
Flash Point 160 °C
320 °F
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 75.0 °C
0.167 hour

@Temperature 167 °F
Recoat, at 50% humidity
30.0 min

@Temperature 75.0 °C
0.500 hour

@Temperature 167 °F
Dust Free, at 50% humidity
180 min

@Temperature 75.0 °C
3.00 hour

@Temperature 167 °F
Dry to handle, at 50% humidity and 75°C
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Evaporation Rate Slower than ether
Flexibility 1/8" conical mandrel
Gloss Retention >90%; 1000 hours QUV
Pencil Hardness 4H
Salt Spray 1000 hours
Solvent Resistance lacquer thinner, acetone, MEK, gasoline, xylene-100double rubs with saturated cloth.
Theoretical Coverage 802 ft2 at 1 mil
Vapor Density Heavier than air