Thermal Properties Metric English Comments
Flash Point 630 °C
1170 °F
ASTM D1929
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures..
Flash Point 630 °C
1170 °F
ASTM D1929
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite
Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is..
Flash Point 630 °C
1170 °F
ASTM D1929
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke
Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C..
Flash Point 630 °C
1170 °F
ASTM D1929
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures..
Flash Point 630 °C
1170 °F
ASTM D1929
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite
Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is..
Flash Point 630 °C
1170 °F
ASTM D1929
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke
Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C..