Polymer Property : Flash Point = 144 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point >= 62.0 °C
>= 144 °F
in a closed crucible
Kazanorgsintez Phenol Resin
Phenol resin is a by-product of phenol and acetone production by the cumene method.Application: Phenol resin is used in the production of phenol-formaldehyde resins and commercial hydrocarbon as a r..
Flash Point 62.0 °C
144 °F
Abel Closed Cup
LyondellBasell PNB Propylene glycol normal butyl ether
Information provided by Lyondell.
Flash Point 62.0 °C
144 °F
Tag Closed Cup; ASTM D56
Chesterton 274 Industrial Degreaser
Description: Chesterton® 274 Industrial Degreaser is an industrial strength, hard surface degreaser which will dissolve grease, oil, tar and other similar water insoluble soils generally encountere..
Flash Point 62.2 °C
144 °F
ASTM D56
ExxonMobil Isopar™ L (AM) Isoparaffin Fluid
Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Central America, South Amer..
Flash Point 62.0 °C
144 °F
Chesterton 706 FG Rustsalvo®
Description: Chesterton® 706 FG Rustsolvo is a high quality, fast acting, penetrating oil which reaches deeply in and frees frozen nuts, bolts, and fittings without injury to the base metal. Due to..
Flash Point 62.0 °C
144 °F
closed cup
Dow Corning Z-6403 SILANE
Dow Corning® Z-6403 Silane is high purity, undiluted isobutyltriethoxy-silane. When diluted with an appropriate solvent, it can be used in the formulation of water repellent products. Upon proper a..
Flash Point 62.0 °C
144 °F
Closed Cup
3M CC-2 Cable Cleaning Preparation Kits
3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form..
Flash Point 62.0 °C
144 °F
Closed Cup
3M CC-3 Cleaning Pad Kits
3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form..
Flash Point 62.0 °C
144 °F
Closed Cup
3M CC-4 Cleaning Solvent
3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form..
Flash Point 62.0 °C
144 °F
Chesterton 723 FG Sprasolvo®
Description: Chesterton® 723 FG Sprasolvo is a high quality, fast acting, penetrating oil which reaches deeply in and frees frozen nuts, bolts, and fittings without injury to the base metal. Due to..