Thermal Properties Metric English Comments
Flash Point 18.0 °C
64.4 °F
Lord Adhesives 204 Semi-Flexible, Medium Cure, High Viscosity Acrylic Adhesive
Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f..
Flash Point 18.0 °C
64.4 °F
Seta
Lord Adhesives Flocklok® 850 Flock Adhesive
Flocklok® 850 is a moisture curing, polyurethane flock adhesive. It is used to adhere flock to SBR elastomers, thermoplastic elastomers, and plastics (i.e., ABS). Thermoplastic elastomers will re..
Flash Point 18.0 °C
64.4 °F
Seta
Lord Adhesives Flocklok® 851 Flock Adhesive
Flocklok® 851 is a moisture curing, polyurethane flock adhesive used to adhere flock to SBR, thermoplastic elastomers, and plastic (i.e., ABS). Thermoplastic elastomers will require the use of a ..
Flash Point 18.0 °C
64.4 °F
Lord Adhesives 201 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive
Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f..