Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lord Adhesives 204 Semi-Flexible, Medium Cure, High Viscosity Acrylic Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Lord Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives 204 Semi-Flexible, Medium Cure, High Viscosity Acrylic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range from paste to liquid. Cure times range from 2 to 35 minutes.Lord Adhesives 204 Semi-Flexible, Medium Cure, High Viscosity Acrylic Adhesive
Physical Properties Metric English Comments
Density 1.02 - 1.04 g/cc
0.0368 - 0.0377 lb/in³
Viscosity 100000 - 300000 cP
100000 - 300000 cP
Thermal Properties Metric English Comments
Flash Point 18.0 °C
64.4 °F
Processing Properties Metric English Comments
Cure Time 120 min
2.00 hour
Pot Life 6.0 - 8.0 min
6.0 - 8.0 min
Time before parts must be mated
Descriptive Properties Value Comments
Color Off-White
Users viewing this material also viewed the following: