Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 18.0 °C | 64.4 °F | |
Lord Adhesives 204 Semi-Flexible, Medium Cure, High Viscosity Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Flash Point | 18.0 °C | 64.4 °F | Seta |
Lord Adhesives Flocklok® 850 Flock Adhesive Flocklok® 850 is a moisture curing, polyurethane flock adhesive. It is used to adhere flock to SBR elastomers, thermoplastic elastomers, and plastics (i.e., ABS). Thermoplastic elastomers will re.. |
|||
Flash Point | 18.0 °C | 64.4 °F | Seta |
Lord Adhesives Flocklok® 851 Flock Adhesive Flocklok® 851 is a moisture curing, polyurethane flock adhesive used to adhere flock to SBR, thermoplastic elastomers, and plastic (i.e., ABS). Thermoplastic elastomers will require the use of a .. |
|||
Flash Point | 18.0 °C | 64.4 °F | |
Lord Adhesives 201 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |