Thermal Properties Metric English Comments
CTE, linear 250 µm/m-°C
139 µin/in-°F
ASTM E831
Parker Chomerics THERM-A-FORM T646 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
CTE, linear 250 - 250 µm/m-°C

@Temperature 70.0 - 150 °C
139 - 139 µin/in-°F

@Temperature 158 - 302 °F
Average value: 250 µm/m-°C Grade Count:2
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..
CTE, linear 250 µm/m-°C
139 µin/in-°F
Alpha 2
Lord Adhesives Thermosetâ„¢ MD-110 Conductive Adhesive
LORD Thermosetâ„¢ MD-110 silver-filled conductive adhesive offers excellent electrical conductivity and room temperature stability. It is designed for use with automated dispensing, stamping and..
CTE, linear 250 µm/m-°C

@Temperature 20.0 °C
139 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials RTV11 White General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
CTE, linear 250 µm/m-°C

@Temperature 20.0 °C
139 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials RTV8111 Silicone Rubber Compounds for Potting, Encapsulating and Sealing
RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr..
CTE, linear 250 µm/m-°C

@Temperature 20.0 °C
139 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials RTV8111 White General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
CTE, linear 250 µm/m-°C

@Temperature 20.0 °C
139 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials RTV8112 Silicone Rubber Compounds for Potting, Encapsulating and Sealing
RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr..
CTE, linear 250 µm/m-°C

@Temperature 20.0 °C
139 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials RTV8112 White General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
CTE, linear 250 µm/m-°C

@Temperature 20.0 °C
139 µin/in-°F

@Temperature 68.0 °F
Momentive Performance Materials RTV567 Translucent Extreme Low Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
CTE, linear 250 µm/m-°C

@Temperature 20.0 °C
139 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Micropol Isoplas P602 Crosslinkable Polyethylene
Information provided by Micropol Limited