Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.0 - 250 µm/m-°C | 7.78 - 139 µin/in-°F | Average value: 107 µm/m-°C Grade Count:46 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
CTE, linear | 140 - 250 µm/m-°C @Temperature 100 - 200 °C |
77.8 - 139 µin/in-°F @Temperature 212 - 392 °F |
Average value: 195 µm/m-°C Grade Count:1 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
CTE, linear | 250 - 250 µm/m-°C @Temperature 70.0 - 150 °C |
139 - 139 µin/in-°F @Temperature 158 - 302 °F |
Average value: 250 µm/m-°C Grade Count:2 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |