Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 139 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 14.0 - 250 µm/m-°C
7.78 - 139 µin/in-°F
Average value: 107 µm/m-°C Grade Count:46
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
CTE, linear 140 - 250 µm/m-°C

@Temperature 100 - 200 °C
77.8 - 139 µin/in-°F

@Temperature 212 - 392 °F
Average value: 195 µm/m-°C Grade Count:1
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
CTE, linear 250 - 250 µm/m-°C

@Temperature 70.0 - 150 °C
139 - 139 µin/in-°F

@Temperature 158 - 302 °F
Average value: 250 µm/m-°C Grade Count:2
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..