Thermal Properties Metric English Comments
CTE, linear 5.30 µm/m-°C
2.94 µin/in-°F
Plansee DENSIMET® D2M Tungsten-Nickel-Molybdenum-Iron Alloy
Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d..
CTE, linear 5.30 µm/m-°C
2.94 µin/in-°F
at Set Pt. (Fired Thermal Expansion)
Ferro EG 2000 Low-Temperature Sealing
VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp..
CTE, linear 5.30 µm/m-°C

@Temperature 25.0 - 600 °C
2.94 µin/in-°F

@Temperature 77.0 - 1110 °F
ICE Mullite, 3Al2O3-SiO2
Data provided by the manufacturer, International Ceramic Engineering.
CTE, linear 5.30 µm/m-°C

@Temperature 25.0 - 260 °C
2.94 µin/in-°F

@Temperature 77.0 - 500 °F
Ferro EG 2810 Dental Glass
Glass Type: Ba-Al-B-Si Typical Application: Glass Filler Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro also manufacture..
CTE, linear 5.30 µm/m-°C

@Temperature 20.0 - 1000 °C
2.94 µin/in-°F

@Temperature 68.0 - 1830 °F
Goodfellow TZM Molybdenum High Temperature Alloy
Increased high temperature strength over pure molybdenum although, like Molybdenum, it oxidizes rapidly in oxidizing atmospheres above 500°CInformation provided by Goodfellow.
CTE, linear 5.30 µm/m-°C

@Temperature 25.0 - 1000 °C
2.94 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek Mullite, S2
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 5.30 µm/m-°C

@Temperature 1000 °C
2.94 µin/in-°F

@Temperature 1830 °F
Chosun Refractories H-3 High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.30 µm/m-°C

@Temperature 1000 °C
2.94 µin/in-°F

@Temperature 1830 °F
Chosun Refractories N3-1 Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.30 µm/m-°C

@Temperature 1000 °C
2.94 µin/in-°F

@Temperature 1830 °F
Chosun Refractories N3-2 Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.30 µm/m-°C

@Temperature 1000 °C
2.94 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SAL60 Special Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.30 µm/m-°C

@Temperature 100 - 1100 °C
2.94 µin/in-°F

@Temperature 212 - 2010 °F
3M Nextel™ 440 Industrial Ceramic Fiber
Chemical composition above is wt%. Crystal phases are gamma alumina + mullite + amorphous SiO2. Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural ap..
CTE, linear 5.30 µm/m-°C

@Temperature 100 - 1100 °C
2.94 µin/in-°F

@Temperature 212 - 2010 °F
3M Nextel™ 550 Industrial Ceramic Fiber
Chemical composition above is wt%. Crystal phases are gamma alumina amorphous SiO2. Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural applications w..
CTE, linear 5.30 µm/m-°C

@Temperature 100 - 1100 °C
2.94 µin/in-°F

@Temperature 212 - 2010 °F
3M Nextel™ CF-40 Woven Fabric 550
Information provided by 3M
CTE, linear 5.30 µm/m-°C

@Temperature 100 - 1100 °C
2.94 µin/in-°F

@Temperature 212 - 2010 °F
3M Nextel™ BF-30 Woven Fabric 440
Information provided by 3M
CTE, linear 5.30 µm/m-°C

@Temperature 100 - 1100 °C
2.94 µin/in-°F

@Temperature 212 - 2010 °F
3M Nextel™ BF-20 Woven Fabric 440
Information provided by 3M
CTE, linear 5.30 µm/m-°C

@Temperature 100 - 1100 °C
2.94 µin/in-°F

@Temperature 212 - 2010 °F
3M Nextel™ BF-40 Woven Fabric 440
Information provided by 3M