Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® D02 PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® D02TS PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® D03 PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® D05 PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® DET PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® HS240 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® HS260 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® HT135 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® HT200 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® HT230 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® HT270 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® HT55 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® HT80 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® LLS215 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® LS200 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® LS230 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
CTE, linear | 367 µm/m-°C | 204 µin/in-°F | converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C |
Solvay Specialty Polymers Galden® HT110 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service tem.. |