Thermal Properties Metric English Comments
CTE, linear 60.0 - 400 µm/m-°C
33.3 - 222 µin/in-°F
Average value: 117 µm/m-°C Grade Count:6
Overview of materials for PEN-PET
This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent..
CTE, linear 13.0 - 400 µm/m-°C
7.22 - 222 µin/in-°F
Average value: 60.2 µm/m-°C Grade Count:46
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
CTE, linear 19.8 - 400 µm/m-°C
11.0 - 222 µin/in-°F
Average value: 73.1 µm/m-°C Grade Count:13
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
CTE, linear 350 - 400 µm/m-°C
194 - 222 µin/in-°F
Master Bond MasterSil 153Med Silicone Paste for Medical Applications
Description: Master Bond MasterSil 153Med is a two component silicone compound with a paste consistency for high performance bonding and sealing. It can be used for medical device applications as it..