Thermal Properties Metric English Comments
CTE, linear 335 µm/m-°C
186 µin/in-°F
Silicone Property; ASTM E 831
Arlon R36798T017 0.017" (0.432 mm) Uncured Silicone Rubber with Laminated Tefzel® Substrate  (discontinue
Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionAppearance: Translucent, high viscosity gum on fluoro..
CTE, linear 335 µm/m-°C

@Temperature 20.0 °C
186 µin/in-°F

@Temperature 68.0 °F
Silicone Property; ASTM E 831
Arlon 25188T010 Silicone Rubber/Laminated ETFE Film
Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion
CTE, linear 335 µm/m-°C

@Temperature 20.0 °C
186 µin/in-°F

@Temperature 68.0 °F
Silicone Property; ASTM E 831
Arlon 25188T017 Silicone Rubber/Laminated ETFE Film
Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion
CTE, linear 335 µm/m-°C
186 µin/in-°F
Silicone Property; Arlon SQA-TMS-022
Arlon 25188T020 0.020" Uncured Silicone Rubber/Laminated ETFE Film
Design/Construction:Liner: 0.003" PTFE Coated FiberglassSide 1: Uncured Silicone RubberSubstrate: Laminated ETFE Film-treated for adhesionThis data represents typical values for the production ma..
CTE, linear 335 µm/m-°C
186 µin/in-°F
Silicone Property; ASTM E 831
Arlon R37208T017 0.017" (0.432 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Liner
Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionThis data represents typical values for the productio..
CTE, linear 335 µm/m-°C
186 µin/in-°F
Silicone Property; ASTM E 831
Arlon R37230R006 0.006" (0.152 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate
Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substrate: PTFE Coated Fiberglass This data represents typical values for the production material. The data should not be used to wri..
CTE, linear 335 µm/m-°C

@Temperature 20.0 °C
186 µin/in-°F

@Temperature 68.0 °F
silicone property; ASTM E 831
Arlon Thermabond® 99180T010 Silicone Rubber/Fiberglass Laminate