Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon R37230R006 0.006" (0.152 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R37230R006 0.006" (0.152 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substrate: PTFE Coated Fiberglass This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns
1.00 mil
152 microns
6.00 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 18
18
Silicone Property; ASTM D2240
Tensile Strength 6.89 MPa
1000 psi
Silicone Property; ASTM D412
Elongation at Break 950 %
950 %
Silicone Property; ASTM D412
Modulus of Elasticity 0.000517 GPa
0.0750 ksi
Silicone Property; ASTM E 831
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Shear Strength 3.96 MPa
575 psi
Arlon SQA-TMS-018
Thermal Properties Metric English Comments
CTE, linear 335 µm/m-°C
186 µin/in-°F
Silicone Property; ASTM E 831
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
Silicone Property; Arlon SQA-TMS-022
Maximum Service Temperature, Air 204.0 °C
399.2 °F
Minimum Service Temperature, Air -136 °C
-212 °F
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure 0.103 - 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 15.0 - 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 4.00 - 10.0 °C
6.00 Month

@Temperature 39.2 - 50.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (g/m2) 175
Arlon SQA-TMS-025
Users viewing this material also viewed the following: