Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 117 - 171 µm/m-°C | 65.0 - 95.0 µin/in-°F | Average value: 150 µm/m-°C Grade Count:15 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsubishi Iupilon® H2000R 23 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsubishi Iupilon® H2000UR 23 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsubishi Iupilon® H2001R 23 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsubishi Iupilon® H3000R 30 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsubishi Iupilon® H3000UR 30 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsubishi Iupilon® S2000R 9.5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsubishi Iupilon® S3000R 16.5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsubishi Iupilon® S3000UR 16.5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsubishi Iupilon® S3001R 16.5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Saint-Gobain Norton® PMP Film Features/Benefits:Good release properties for up to 180°C (356°F) cure composites (application dependent)low density for high surface area per poundExcellent clarityThermoformableProduct avail.. |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Kynar® 740 PVDF Homopolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Pomalux® SD-A Acetal Copolymer (anti-static) Non-carbon-filled, permanently static-dissipative material which is non-migratory and non-humidity dependent. With enhanced lubricity, POMALUX SD-A provides superior wear resistance and ease of mac.. |
|||
CTE, linear | 117 µm/m-°C | 65.0 µin/in-°F | ASTM E831 |
Goodfellow TPX® DX350 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
CTE, linear | 117 µm/m-°C | 65.0 µin/in-°F | ASTM E831 |
Goodfellow TPX® MX002O Polymethylpentene This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi.. |
|||
CTE, linear | 117 µm/m-°C | 65.0 µin/in-°F | ASTM E831 |
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
CTE, linear | 117 µm/m-°C | 65.0 µin/in-°F | ASTM E831 |
Goodfellow TPX® DX231 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
CTE, linear | 117 µm/m-°C | 65.0 µin/in-°F | ASTM E831 |
Goodfellow TPX® DX310 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
CTE, linear | 117 µm/m-°C | 65.0 µin/in-°F | ASTM E831 |
Goodfellow TPX® DX845 Extrusion Grade Polymethylpentene This grade is highly recommended for film extrusion; also for injection molding, fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensiv.. |
|||
CTE, linear | 117 µm/m-°C | 65.0 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® EM127 Electrically Conductive Epoxy Product Description: EPO-TEK® EM127 is a single component, heat curable, electrically conductive epoxy adhesive for semiconductor IC and LED die attach applications.Advantages & Application Notes: .. |
|||
CTE, linear | 117 µm/m-°C @Temperature -30.0 - 30.0 °C |
65.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8254 HS BK-102 PA6 (Dry) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
CTE, linear | 117 µm/m-°C | 65.0 µin/in-°F | Average value: 117 µm/m-°C Grade Count:7 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
|
Dow Pellethane® 2354-65D Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2354-65D elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyurethane.. |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsui TPX® DX820 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsui TPX® MX002 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
CTE, linear | 117 µm/m-°C @Temperature 20.0 °C |
65.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Mitsui TPX® MX004 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |