Thermal Properties Metric English Comments
CTE, linear -1.00 - 7.00 µm/m-°C

@Temperature 55.0 - 260 °C
-0.556 - 3.89 µin/in-°F

@Temperature 131 - 500 °F
Average value: 2.88 µm/m-°C Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
CTE, linear -1.00 - 7.00 µm/m-°C

@Thickness 2.00 - 4.00 mm
-0.556 - 3.89 µin/in-°F

@Thickness 0.0787 - 0.157 in
Average value: 2.88 µm/m-°C Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
CTE, linear 6.30 - 7.00 µm/m-°C

@Temperature 20.0 - 100 °C
3.50 - 3.89 µin/in-°F

@Temperature 68.0 - 212 °F
MarkeTech W85Cu Tungsten/Copper Heat Sink Material
WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c..
CTE, linear 6.00 - 7.00 µm/m-°C

@Temperature 1000 °C
3.33 - 3.89 µin/in-°F

@Temperature 1830 °F
Chosun Refractories BPSC-95 Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.00 - 7.00 µm/m-°C
2.78 - 3.89 µin/in-°F
IPC TM-650 2.4.41
Arlon 45NK Woven Kevlar® Reinforced Laminate and Prepreg
45NK is a woven Kevlar® aramid fiber reinforced multifunctional epoxy laminate system engineered to provide in-plane CTE values as low as 6 ppm/°C for compatibility with leadless alumina ceramic c..