Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.00 - 48.0 µm/m-°C | 3.33 - 26.7 µin/in-°F | Average value: 28.7 µm/m-°C Grade Count:3 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
CTE, linear | 6.00 - 144 µm/m-°C @Temperature 50.0 - 300 °C |
3.33 - 80.0 µin/in-°F @Temperature 122 - 572 °F |
Average value: 48.7 µm/m-°C Grade Count:29 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
CTE, linear | 6.00 µm/m-°C @Temperature 23.0 °C |
3.33 µin/in-°F @Temperature 73.4 °F |
MD; ASTM D696 |
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
CTE, linear | 6.00 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
3.33 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP555 Carbon Fiber
(discontinued **) Description: NP555 is composed of carbon fiber fabric and a phenolic resin system. It has excellent moisture resistance and physical properties. This material was designed to replace asbestos vane m.. |
|||
CTE, linear | 6.00 - 73.8 µm/m-°C | 3.33 - 41.0 µin/in-°F | Average value: 50.9 µm/m-°C Grade Count:41 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
CTE, linear | 6.00 - 25.0 µm/m-°C | 3.33 - 13.9 µin/in-°F | Average value: 16.4 µm/m-°C Grade Count:8 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
CTE, linear | 6.00 - 85.0 µm/m-°C | 3.33 - 47.2 µin/in-°F | Average value: 46.2 µm/m-°C Grade Count:33 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
CTE, linear | 6.00 µm/m-°C @Temperature 260 °C |
3.33 µin/in-°F @Temperature 500 °F |
Fired Thermal Expansion |
Ferro CF 7586 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific t.. |
|||
CTE, linear | 6.00 µm/m-°C @Temperature 20.0 °C |
3.33 µin/in-°F @Temperature 68.0 °F |
|
MarkeTech Strontium Lanthanum Galate (SrLaGaO3) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |
|||
CTE, linear | 6.00 µm/m-°C | 3.33 µin/in-°F | at Set Pt.; Crystallized |
Ferro EG 2928 Glaze and Sealant Glass Glass Type: Pb-Zn-B Typical Powder Form: VEG, MVG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective an.. |
|||
CTE, linear | 6.00 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.33 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott G018-161 Dental Glass Remarks: Extremely high radioopacity, Zr containingApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provide.. |
|||
CTE, linear | 6.00 µm/m-°C @Temperature 1000 °C |
3.33 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories BP-95A Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 6.00 - 7.00 µm/m-°C @Temperature 1000 °C |
3.33 - 3.89 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories BPSC-95 Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 6.00 µm/m-°C @Temperature 1000 °C |
3.33 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories H-2 High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 6.00 µm/m-°C @Temperature 1000 °C |
3.33 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SF32 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 6.00 µm/m-°C @Temperature 1000 °C |
3.33 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SF-S Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 6.00 µm/m-°C | 3.33 µin/in-°F | |
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
CTE, linear | 6.00 µm/m-°C @Temperature 20.0 - 1093 °C |
3.33 µin/in-°F @Temperature 68.0 - 1999 °F |
|
BNZ Materials Zelieblok 1900S Structural Ceramic Insulation Information provided by BNZ Materials Inc. |
|||
CTE, linear | 6.00 - 9.00 µm/m-°C | 3.33 - 5.00 µin/in-°F | IPC TM-650 2.4.41 |
Arlon 85NT Polyimide Nonwoven Aramid Laminate and Prepreg 85NT is a pure polyimide laminate and prepreg system (Tg = 250°C), reinforced with a non-woven aramid substrate. This system combines the high-reliability features of polyimide (improved PTH relia.. |
|||
CTE, linear | 6.00 µm/m-°C @Temperature 100 - 1100 °C |
3.33 µin/in-°F @Temperature 212 - 2010 °F |
|
3M Nextel™ 720 Composite Ceramic Fiber Chemical composition above is wt%. Filament diameter is 10-12 µm.3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 .. |
|||
CTE, linear | 6.00 µm/m-°C @Temperature 20.0 °C |
3.33 µin/in-°F @Temperature 68.0 °F |
|
ATI Wah Chang Zirconium Alloy Zircaloy-4 Zirconium resists corrosive attack in most organic and mineral acids, strong alkalis, and some molten salts. A tightly adherent and protective oxide film protects the metal-oxide interface to provid.. |
|||
CTE, linear | 6.00 µm/m-°C @Temperature 100 - 1100 °C |
3.33 µin/in-°F @Temperature 212 - 2010 °F |
|
3M Nextel™ XN-513 Woven Fabric 720 Information provided by 3M |
|||
CTE, linear | 6.00 µm/m-°C | 3.33 µin/in-°F | at Set Pt. |
Ferro EG 2800 Metal Sealing Glass Type: CA-Si-B Typical Powder Form: VSD Typical Application: TA 23 Battery Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se.. |
|||
CTE, linear | 6.00 µm/m-°C @Temperature 20.0 °C |
3.33 µin/in-°F @Temperature 68.0 °F |
|
Mateck Thallium Bromoiodide TIBr-TII (KRS-5) Optical crystals |