Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.50 - 7.80 µm/m-°C @Temperature 25.0 - 800 °C |
3.61 - 4.33 µin/in-°F @Temperature 77.0 - 1470 °F |
|
China-Yixing Longly Refractories 95 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
CTE, linear | 6.50 - 7.80 µm/m-°C @Temperature 25.0 - 800 °C |
3.61 - 4.33 µin/in-°F @Temperature 77.0 - 1470 °F |
|
China-Yixing Longly Refractories 95 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |