Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco 400 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco ASPECT® 3000 Wollastonite High aspect ratio grade. It is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. .. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco ASPECT® 4000 Wollastonite ASPECT 4000 is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive .. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco HARRP™ 20 X 40 Wollastonite HARRP™ 20X40 is suggested for concrete and concrete roof tile reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco HARRP™ 40 Wollastonite HARRP™ 40 is suggested for concrete, roof tile, grout/stucco, etc. reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distin.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M1250 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M15 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M3 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD G® WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 20.0 °C |
3.61 µin/in-°F @Temperature 68.0 °F |
|
Nyco NYAD® G Special Wollastonite Wollastonite (calcium metasilicate, or CaSiO3) is a naturally occurring white, non-metallic mineral with an acicular or needle-shaped crystal structure. This distinctive property makes wollastonite .. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® G Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® M100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® M1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® M400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® MD1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® MD200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® MD325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® MD400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® MG Wollastonite High aspect ratio grade. This grade is recommended for elastomer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinct.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYCOR® R Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® 12 Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M15 Wollastonite High aspect ratio grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal perf.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M50 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 20.0 °C |
3.61 µin/in-°F @Temperature 68.0 °F |
|
MarkeTech WCu10 Tungsten Copper Alloy Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 260 °C |
3.61 µin/in-°F @Temperature 500 °F |
|
Ferro IP 550 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 1000 °C |
3.61 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories H-1 High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 6.50 - 7.10 µm/m-°C @Temperature 20.0 - 1000 °C |
3.61 - 3.94 µin/in-°F @Temperature 68.0 - 1830 °F |
|
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain) LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good .. |