Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco ASPECT® 3000 Wollastonite High aspect ratio grade. It is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. .. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco HARRP™ 40 Wollastonite HARRP™ 40 is suggested for concrete, roof tile, grout/stucco, etc. reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distin.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco HARRP™ Coarse Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M1250 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M15 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M200 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M325 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® 325 Wollastonite Powdered grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particl.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® 400 Wollastonite Chemically treated powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an .. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 20.0 °C |
3.61 µin/in-°F @Temperature 68.0 °F |
|
Nyco NYAD® G Special Wollastonite Wollastonite (calcium metasilicate, or CaSiO3) is a naturally occurring white, non-metallic mineral with an acicular or needle-shaped crystal structure. This distinctive property makes wollastonite .. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® G Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® M400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® MD1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® MG Wollastonite High aspect ratio grade. This grade is recommended for elastomer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinct.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYCOR® 100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® 20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® 4W Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M15 Wollastonite High aspect ratio grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal perf.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M3 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M50 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 260 °C |
3.61 µin/in-°F @Temperature 500 °F |
|
Ferro IP 550 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |
|||
CTE, linear | 6.50 - 7.10 µm/m-°C @Temperature 20.0 - 1000 °C |
3.61 - 3.94 µin/in-°F @Temperature 68.0 - 1830 °F |
|
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain) LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good .. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco 10 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 - 7.80 µm/m-°C @Temperature 25.0 - 800 °C |
3.61 - 4.33 µin/in-°F @Temperature 77.0 - 1470 °F |
|
China-Yixing Longly Refractories 95 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature -60.0 - 60.0 °C |
3.61 µin/in-°F @Temperature -76.0 - 140 °F |
|
Mateck Zinc Sulfide Cleartran (ZnS) Optical Crystals |