Polymer Property : CTE, linear = 71.1 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 128 µm/m-°C
71.1 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® M10-D Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..
CTE, linear 128 µm/m-°C
71.1 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® MA-5 Optical Grade Epoxy
Material Description: A single component, B-stageable, optical grade epoxy for fiber optic assembly. It may be used for B-stage sealing of fiber cables into ferrules, or fiber optic feed through in..
CTE, linear 128 µm/m-°C
71.1 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® OE138 Two Component Epoxy
Material Description: A two component epoxy with intermediate viscosity range between EPO-TEK® 353ND and EPO-TEK® 353ND-T. It is designed for semiconductor glob top applications, as well as use in..
CTE, linear 128 µm/m-°C
71.1 µin/in-°F
Silicone Property; ASTM E 831
Arlon Thermabond® 99A60X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
CTE, linear 128 µm/m-°C
71.1 µin/in-°F
Silicone Property; ASTM E831
Arlon Thermabond® R37300X008 0.008" Uncured Silicone Rubber on Fiberglass Carrier
Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m..
CTE, linear 128 µm/m-°C

@Temperature 20.0 °C
71.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products  (discontinued **)
Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin that has outstanding resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated s..