Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon Thermabond® R37300X008 0.008" Uncured Silicone Rubber on Fiberglass Carrier

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Thermabond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® R37300X008 0.008" Uncured Silicone Rubber on Fiberglass Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 mil PTFE coated fiberglassThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 2.60 g/cc
0.0939 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 203 microns
8.00 mil
Product; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
Silicone Property; ASTM D2240
Tensile Strength 2.28 MPa
330 psi
Silicone Property; ASTM D412
Elongation at Break 170 %
170 %
Silicone Property; ASTM D412
Modulus of Elasticity 0.00159 GPa
0.230 ksi
Silicone Property; Arlon SQA-TMS-008
Poissons Ratio 0.50
0.50
Shear Modulus <= 0.000345 GPa
<= 0.0500 ksi
Product Property; ASTM D1002
Shear Strength 2.07 MPa
300 psi
Lap; Product Property; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 128 µm/m-°C
71.1 µin/in-°F
Silicone Property; ASTM E831
Specific Heat Capacity 0.900 J/g-°C
0.215 BTU/lb-°F
Silicone Property; ASTM E1461-01
Thermal Conductivity 1.70 W/m-K

@Temperature 100 °C
11.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; ASTM E1530
Maximum Service Temperature, Inert 204 °C
399 °F
Minimum Service Temperature, Air -100 °C
-148 °F
Glass Transition Temp, Tg -120 °C
-184 °F
Silicone Property; ASTM D3418
Electrical Properties Metric English Comments
Dielectric Constant 5.9

@Frequency 1.00e+6 Hz
5.9

@Frequency 1.00e+6 Hz
Silicone Property; IPC TM 650 - 2.5.5.3
Dielectric Strength 41.3 kV/mm
1050 kV/in
ASTM D149
Dissipation Factor 0.0040

@Frequency 1.00e+6 Hz
0.0040

@Frequency 1.00e+6 Hz
Silicone Property; IPC TM 650 - 2.5.5.3
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 100 °C
0.250 hour

@Temperature 212 °F
Recommended Cure Cycle; After Thermabond® reaches temperature
Shelf Life 6.00 Month

@Temperature 7.22 °C
6.00 Month

@Temperature 45.0 °F
Descriptive Properties Value Comments
Color Gray
Plasticity (mm) 2.2
Arlon SQA-TMS-005
Thermal Resistance (°C-in2/W) 0.112
ASTM E1530
Total Product Weight (oz/yd2) 15.5
Arlon SQA-TMS-025
Users viewing this material also viewed the following: