Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0300 W/m-K @Temperature 200 °C |
0.208 BTU-in/hr-ft²-°F @Temperature 392 °F |
Arlon SQA-TMS-022 |
Arlon 680-R3844R 0.084" (2.13 mm) Cured Silicone Coating with Silica-based Substrate Design/Construction:Side 1: Cured Silicone Coating Substrate: Silica-basedSide 2: Cured Silicone Coating Rubber Application Advantages:Extremely low thermal conductivityThermally stableBondable to s.. |
|||
Thermal Conductivity | 0.0300 W/m-K @Temperature -20.0 °C |
0.208 BTU-in/hr-ft²-°F @Temperature -4.00 °F |
|
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0300 - 0.316 W/m-K | 0.208 - 2.19 BTU-in/hr-ft²-°F | according to the difference density |
Beijing Evergrow Resources BF-10 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thermal Conductivity | 0.0300 - 0.316 W/m-K | 0.208 - 2.19 BTU-in/hr-ft²-°F | according to the difference density |
Beijing Evergrow Resources BF-25 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thermal Conductivity | 0.0300 W/m-K @Temperature -20.0 °C |
0.208 BTU-in/hr-ft²-°F @Temperature -4.00 °F |
|
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0300 W/m-K @Thickness 50.0 mm, Temperature -20.0 °C |
0.208 BTU-in/hr-ft²-°F @Thickness 1.97 in, Temperature -4.00 °F |
|
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0300 - 0.316 W/m-K | 0.208 - 2.19 BTU-in/hr-ft²-°F | according to the difference density |
Beijing Evergrow Resources BF-15 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thermal Conductivity | 0.0300 - 0.316 W/m-K | 0.208 - 2.19 BTU-in/hr-ft²-°F | according to the difference density |
Beijing Evergrow Resources BF-20 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thermal Conductivity | 0.0300 - 0.316 W/m-K | 0.208 - 2.19 BTU-in/hr-ft²-°F | according to the difference density |
Beijing Evergrow Resources BF-3 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thermal Conductivity | 0.0300 - 0.316 W/m-K | 0.208 - 2.19 BTU-in/hr-ft²-°F | according to the difference density |
Beijing Evergrow Resources BF-6 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thermal Conductivity | 0.0300 - 0.180 W/m-K | 0.208 - 1.25 BTU-in/hr-ft²-°F | Average value: 0.0389 W/m-K Grade Count:9 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Thermal Conductivity | 0.0300 W/m-K @Temperature -20.0 °C |
0.208 BTU-in/hr-ft²-°F @Temperature -4.00 °F |
|
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0300 W/m-K @Thickness 20.0 mm |
0.208 BTU-in/hr-ft²-°F @Thickness 0.787 in |
DIN EN 13164 |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0300 W/m-K @Temperature -20.0 °C |
0.208 BTU-in/hr-ft²-°F @Temperature -4.00 °F |
|
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0300 W/m-K @Thickness 20.0 mm |
0.208 BTU-in/hr-ft²-°F @Thickness 0.787 in |
DIN EN 13164 |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0300 W/m-K @Temperature -20.0 °C |
0.208 BTU-in/hr-ft²-°F @Temperature -4.00 °F |
|
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |