Polymer Property : Thermal Conductivity = 0.208 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0299 W/m-K

@Temperature 24.0 °C
0.208 BTU-in/hr-ft²-°F

@Temperature 75.2 °F
Sharadaa Ceramics Resin Bonded Slabs
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Thermal Conductivity 0.0300 W/m-K

@Temperature 200 °C
0.208 BTU-in/hr-ft²-°F

@Temperature 392 °F
Arlon SQA-TMS-022
Arlon 680-R3844R 0.084" (2.13 mm) Cured Silicone Coating with Silica-based Substrate
Design/Construction:Side 1: Cured Silicone Coating Substrate: Silica-basedSide 2: Cured Silicone Coating Rubber Application Advantages:Extremely low thermal conductivityThermally stableBondable to s..
Thermal Conductivity 0.0300 W/m-K

@Temperature -20.0 °C
0.208 BTU-in/hr-ft²-°F

@Temperature -4.00 °F
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0300 - 0.316 W/m-K
0.208 - 2.19 BTU-in/hr-ft²-°F
according to the difference density
Beijing Evergrow Resources BF-10 Basalt Needle Felt
Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi..
Thermal Conductivity 0.0300 - 0.316 W/m-K
0.208 - 2.19 BTU-in/hr-ft²-°F
according to the difference density
Beijing Evergrow Resources BF-25 Basalt Needle Felt
Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi..
Thermal Conductivity 0.0300 W/m-K

@Temperature -20.0 °C
0.208 BTU-in/hr-ft²-°F

@Temperature -4.00 °F
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0300 W/m-K

@Thickness 50.0 mm,
Temperature -20.0 °C
0.208 BTU-in/hr-ft²-°F

@Thickness 1.97 in,
Temperature -4.00 °F
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0300 - 0.316 W/m-K
0.208 - 2.19 BTU-in/hr-ft²-°F
according to the difference density
Beijing Evergrow Resources BF-15 Basalt Needle Felt
Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi..
Thermal Conductivity 0.0300 - 0.316 W/m-K
0.208 - 2.19 BTU-in/hr-ft²-°F
according to the difference density
Beijing Evergrow Resources BF-20 Basalt Needle Felt
Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi..
Thermal Conductivity 0.0300 - 0.316 W/m-K
0.208 - 2.19 BTU-in/hr-ft²-°F
according to the difference density
Beijing Evergrow Resources BF-3 Basalt Needle Felt
Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi..
Thermal Conductivity 0.0300 - 0.316 W/m-K
0.208 - 2.19 BTU-in/hr-ft²-°F
according to the difference density
Beijing Evergrow Resources BF-6 Basalt Needle Felt
Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi..
Thermal Conductivity 0.0300 - 0.180 W/m-K
0.208 - 1.25 BTU-in/hr-ft²-°F
Average value: 0.0389 W/m-K Grade Count:9
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Thermal Conductivity 0.0300 W/m-K

@Temperature -20.0 °C
0.208 BTU-in/hr-ft²-°F

@Temperature -4.00 °F
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0300 W/m-K

@Thickness 20.0 mm
0.208 BTU-in/hr-ft²-°F

@Thickness 0.787 in
DIN EN 13164
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0300 W/m-K

@Temperature -20.0 °C
0.208 BTU-in/hr-ft²-°F

@Temperature -4.00 °F
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0300 W/m-K

@Thickness 20.0 mm
0.208 BTU-in/hr-ft²-°F

@Thickness 0.787 in
DIN EN 13164
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0300 W/m-K

@Temperature -20.0 °C
0.208 BTU-in/hr-ft²-°F

@Temperature -4.00 °F
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..