Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.121 W/m-K | 0.840 BTU-in/hr-ft²-°F | |
Trelleborg AEM Syntac® 350 Syntactic Foam Syntac® 350 is made from high grade epoxy resin and hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling.Available in block, sheet and ro.. |
|||
Thermal Conductivity | 0.121 W/m-K | 0.840 BTU-in/hr-ft²-°F | |
Trelleborg AEM Syntac® 351 Syntactic Foam Syntac® 351 is a castable syntactic composite material of epoxy resin and high performance hollow glass microspheres designed specifically for molding thermoforming plugs and other associated tooli.. |