Polymer Property : Thermal Conductivity = 0.840 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.121 W/m-K
0.840 BTU-in/hr-ft²-°F
Trelleborg AEM Syntac® 350 Syntactic Foam
Syntac® 350 is made from high grade epoxy resin and hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling.Available in block, sheet and ro..
Thermal Conductivity 0.121 W/m-K
0.840 BTU-in/hr-ft²-°F
Trelleborg AEM Syntac® 351 Syntactic Foam
Syntac® 351 is a castable syntactic composite material of epoxy resin and high performance hollow glass microspheres designed specifically for molding thermoforming plugs and other associated tooli..