Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.197 W/m-K | 1.36 BTU-in/hr-ft²-°F | |
Honeywell ACLAR® 33C (7.80 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Thermal Conductivity | 0.197 W/m-K | 1.36 BTU-in/hr-ft²-°F | |
Honeywell ACLAR® 33C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Thermal Conductivity | 0.197 W/m-K | 1.37 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® KU 2-7609 Polycarbonate + PBT, Mineral Filled Impact Grade ISO 7792-1-PC/PBT,MHPR,-030,MD20(PC+PBT)-blendsimpact modifiedInjection molding grade20% mineral filledPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.197 W/m-K | 1.37 BTU-in/hr-ft²-°F | |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |